About ceria33
SEM (Tescan Vega (LMU)) was used to observe the cross-sectional and surface area morphology in the membranes of different NP loadings (Determine 1 and Figure S1). Membranes were damaged in liquid nitrogen to fix the cross-sectional finishes on the membranes and also a voltage of 15–20 Kv at distinctive magnifications was utilized with gold coatin